Home > News > Content

The Main Reasons Affecting The Flatness Of Corrugated Board

Jul 03, 2023

 

1. The types and grades of paper on the surface are different.

There are imported and domestic Kraft paper, imitation Kraft paper, corrugated paper, tea board paper, high-strength corrugated paper, etc., which are also divided into A, B, C, D, E. According to the difference in paper materials, the surface paper is generally better than the inner paper.

2. The main technical parameters of the surface paper are different.

From the perspective of cardboard box performance requirements or cost reduction considerations for users, the paper inside the cardboard box is required to be different, usually:

The quantity of paper on the surface varies. Some types of paper have a larger weight than the inner paper, while others have a smaller weight.

The moisture content of the tissue paper varies. Due to differences in environmental humidity such as the supplier and transportation inventory, some types of surface paper have a higher moisture content than the inner paper, while others have a lower moisture content.

The quantity and moisture content of the surface paper vary. One is that the quantity of the surface paper is greater than that of the inner paper, and the moisture content is greater than or less than that of the inner paper; The second is that the weight of the surface paper is smaller than that of the inner paper, and the moisture content is greater than or less than that of the inner paper.

3. The moisture content of the same batch of paper is different.

One part of the paper has a moisture content greater than the other part of the paper or tube between the two ends, the outer edge and the inner edge; The moisture content on the core side is different.

4. Improper selection and adjustment of the length of the heating surface (wrapping angle) of the paper passing through the preheater, or improper selection or adjustment of the length due to heating of the wrapping angle, which affects the preheating and drying effect.

5. The steam spray device cannot be used correctly or there is no spray device on the device, so the paper humidity cannot be added arbitrarily.

6. Insufficient time for paper to dissipate moisture after preheating, high environmental humidity, poor ventilation, and improper production line speed.

7. Improper and uneven gluing of single sided corrugated machines and gluing machines, resulting in uneven shrinkage of cardboard.

8. Insufficient and unstable steam pressure, damage to drain valves and other accessories, or incomplete drainage of accumulated water in pipelines, resulting in the inability of the preheater to operate normally and stably.

图片⑦

 

Send Inquiry
Contact Us